Materials and methods

Test guideline
Qualifier:
according to
Guideline:
EU Method A.3 (Relative Density)
GLP compliance:
yes
Type of method:
pycnometer method

Test material

Reference
Name:
Unnamed
Type:
Constituent
Type:
Constituent
Details on test material:
Batch No. Kn-Gi 9328-182

Results and discussion

Density
Type:
relative density
Density:
1.22 g/cm³
Temp.:
20 °C

Applicant's summary and conclusion

Conclusions:
The relative density of Kn 172 was determined to D420 = 1.216