Registration Dossier

Data platform availability banner - registered substances factsheets

Please be aware that this old REACH registration data factsheet is no longer maintained; it remains frozen as of 19th May 2023.

The new ECHA CHEM database has been released by ECHA, and it now contains all REACH registration data. There are more details on the transition of ECHA's published data to ECHA CHEM here.

Diss Factsheets

Physical & Chemical properties

Auto flammability

Currently viewing:

Administrative data

Link to relevant study record(s)

Reference
Endpoint:
relative self-ignition temperature (solids)
Type of information:
experimental study
Adequacy of study:
key study
Study period:
01 September 2017 - 12 September 2017
Reliability:
1 (reliable without restriction)
Rationale for reliability incl. deficiencies:
guideline study
Remarks:
Test method according to EEC method A.16. GLP study.
Qualifier:
according to guideline
Guideline:
EU Method A.16 (Relative Self-Ignition Temperature for Solids)
Deviations:
no
GLP compliance:
yes (incl. QA statement)
Key result
Relative self-ignition temperature:
348 °C

At the oven temperature of 348 °C, the sample temperature reaches 400 °C. According to the criteria of the method A.16 the observed phenomenon indicates that the relative self-ignition temperature of the sample is 348 °C. See image attached.

Conclusions:
The relative self-ignition temperature of the tested material is 348ºC according to EU method A.16 criteria.
Executive summary:

The determination of the self-ignition temperature of the tested material was performed according to EU Method A.16 (GLP study). A cube of stainless steel wire mesh was filled with the test item, suspended in the centre of the laboratory oven and heated at a constant rate of 0.5ºC/min until reaching 400ºC. One thermocouple was placed at the centre of the cube and the other between the cube and the oven wall to record the oven temperature. According to the test method, the relative self-ignition temperature of the tested material is 348ºC.

Description of key information

Key study. Test method according to EU Method A.16, GLP study. The relative self-ignition temperature of the tested material is 348ºC.

Key value for chemical safety assessment

Autoflammability / Self-ignition temperature at 101 325 Pa:
348 °C

Additional information

Key study: The determination of the self-ignition temperature of the test item was performed according to EU Method A.16 (GLP study). A cube of stainless steel wire mesh was filled with the test item, suspended in the centre of the laboratory oven and heated at a constant rate of 0.5ºC/min until reaching 400ºC. One thermocouple was placed at the centre of the cube and the other between the cube and the oven wall to record the oven temperature. According to the test method, the relative self-ignition temperature of the tested material is 348ºC.