Registration Dossier

Data platform availability banner - registered substances factsheets

Please be aware that this old REACH registration data factsheet is no longer maintained; it remains frozen as of 19th May 2023.

The new ECHA CHEM database has been released by ECHA, and it now contains all REACH registration data. There are more details on the transition of ECHA's published data to ECHA CHEM here.

Diss Factsheets

Physical & Chemical properties

Stability: thermal, sunlight, metals

Currently viewing:

Administrative data

Link to relevant study record(s)

Description of key information

For both metals tested (carbon steel ST37.2 and aluminium AL7075 the corrosion rates are equal or lower than 0.01 mm/a and no local corrosion like pitting corrosion took place.

Additional information

The tested material is not corrosive to metals according to UN classification for dangerous goods, part III, section 37, class 8.

Justification for classification or non-classification

The substance is not corrosive to metals and hence no classification according to GHS (Regulation EC 1272/2008) is required.